THERMOCOUPLE TYPES

CODE

CONDUCTOR COMBINATIONS

NATIONAL STANDARDS FOR OUTPUT OF THERMOCOUPLE CONDUCTORS
THOSE STANDARDS NOTED IN THIS COLUMN ALL CONFORM WITH EACH OTHER AND ARE BASED UPON IEC584.1:1995 & ITS-90

Approximate Working Temperature Range of  Measuring Junction.  NB. Not Related to wire diameters and conductor insulating material.

+LEG -LEG Continuous Short Term

K

NICKEL-CHROMIUM
Also known as : Chromel*, 
Thermokanthal KP*,Ni-Cr,
T1*,Tophel*

NICKEL-ALUMINIUM
(
MAGNETIC)
Also known as: Ni-Al, Alumel*,
Thermokanthal KN*,T2*,Nial*

 BS EN 60584, 1 Pt4:1996
(Replaces BS 4937 Pt 4)
ANSI/MC96.1
DIN EN 60584,1:1996
NF EN 60584 1:1996
JISC 1602

0 to +1100

-180 to +1350

T

COPPER


COPPER-NICKEL
Also known as: Constantan,
Advance*, Cupron*

BS EN 60584, 1 Pt3:1996
(Replaces BS 4937 Pt 5)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

-185 to +300

-250 to +400

J

IRON
(MAGNETIC)
Also known as: Fe

COPPER-NICKEL
Also known as Constantan
Advance*, Cupron*

BS EN 60584, 1 Pt3:1996
(Replaces BS 4937 Pt 3)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

+20 to +700

-180 to +750

N

NICKEL-CHROMIUM-
SILICON
Also known as: Nicrosil

NICKEL-SILICON-
MAGNESIUM
Also known as: Nisil

BS EN 60584, 1 Pt8:1996
(Replaces BS 4937 Pt 8)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

0 to +800

-40 to +900

E

NICKEL-CHROMIUM
Also known as:Chromel*,
Tophal*,Chromium,Nickel


COPPER-NICKEL
Also known as:Nickel-Copper,
Constantan, Advance*,
Cupron*

BS EN 60584, 1 Pt6:1996
(Replaces BS 4937 Pt 6)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

0 to +1100

-270 to +1300

R

PLATINUM
13% RHODIUM

PLATINUM

BS EN 60584, 1 Pt2:1996
(Replaces BS 4937 Pt 2)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

0 to +1600

-50 to +1750

S

PLATINUM
10% RHODIUM

PLATINUM

BS EN 60584, 1 Pt1:1996
(Replaces BS 4937 Pt 1)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

0 to 1550

-50 to +1750

B

PLATINUM
30% RHODIUM

PLATINUM
6% RHODIUM

BS EN 60584, 1 Pt7:1996
(Replaces BS 4937 Pt 7)
ANSI/MC96.1
DIN EN 60584, 1:1996
NF EN 60584, 1:1996
JISC 1602

+100 to +1600

+100 to +1820

G*

TUNGSTEN

TUNGSTEN
26% RHENIUM

There are no officially recognized
standards for Type G

+20 to +2320

0 to +2600

C*

TUNGSTEN
5% RHENIUM

TUNGSTEN
26% RHENIUM

There are no officially recognized
standards for Type G

+50 to +1820

+20 to +2300

D*

TUNGSTEN
3% RHENIUM

TUNGSTEN
25% RHENIUM

There are no officially recognized
standards for Type G

0 to +2100

0 to +2600

 


Home Page Site Map Section 1 Section 2 Section 3 Section 4
Contact Details  Section 5 Section 6 Section 7 Enquiry


By JPN